Transgranular Stress Corrosion Cracking of Mg alloys AZ91, AZ21 and ZE41
 报告人:
Andrej Atrens
Professor of Materials Engineering, 
Division of Materials, The University of Queensland
报告时间:
2006-09-11 15:30
报告地点:
机械工程系焊接馆 301 房间
主办单位:
机械工程系学术委员会
  简介:

Transgranular Stress Corrosion Cracking of Mg alloys

AZ91, AZ21 and ZE41

 

Andrej Atrens

Professor of Materials Engineering, The University of Queensland, Aus

 

a.atrens@minmet.uq.edu.au

 


Abstract: As the usage of Mg alloys increases in stressed applications, it is worthwhile remembering that many Mg alloys are susceptible to stress corrosion cracking in environments such as distilled water or atmospheric exposure. In the absence of data to the contrary, it is prudent to assume that stress corrosion cracking occurs for stresses above the threshold stress of ~50% of the tensile yield stress.

For AZ91, AZ21 and ZE41 our research aims to compare the critical parameters of TGSCC with a Mg TGSCC model. The TGSCC parameters are the threshold stress for TGSCC, the threshold stress intensity for TGSCC and the crack velocity for TGSCC. The model of Mg TGSCC is based on the most probable mechanism. Hydrogen, released by the cathodic partial reaction at a bare crack tip, diffuses to the stressed region ahead of the crack tip; a brittle hydride precipitates and grows once the hydrogen concentration exceeds the terminal solid solubility; a brittle crack advances through the hydride once the hydride has reached a critical size; the process repeats and the sub-critical crack advances until final fracture occurs when the crack reaches a critical size.

今日相关信息
Failure Analyses of Non-Ceramic Compo...
the Example of Computational Molecula...
 
同类别相关信息
无机有机多孔材料研究
材料学院《材料工程名师讲座》:Carbon...
仿生可控粘附界面材料-清华2018高分子...
(活动时间为3月12日13:00)Provable ...
Nanotechnology for Energy, Environm...
学术活动